Main reasons.
1. lmproper selection ofthinner or excessive use
2. Too low temperature and excessive moisture,resulting in the precipitation ofwater and impuritiesin the clear coat
3. Poor paint quality
4. Polymerization reaction ofpaint base materialreduced solubility, resulting in turbidity
Treatment methods and preventive measures.
1. Add appropriate solvent to improve turbidity
2. Remove water by heating
3. Replace the diluent and choose the appropriatediluent
4. Control the room temperature, the roomtemperature should be kept above 20°C